Brief introduction
Developed for EOR method, is Polyacrylamide with super high molecular weight. Max Molecular weight can be 24 millions.
Technical index:( Company standard: Q/LCL003-2008)
|
Technical index
|
EORPAM-1
|
EORPAM-2
|
EORPAM-3
|
EORPAM-4
|
|
|
20-80
|
|
|
≥89
|
|
|
≤2
|
|
|
≤0.1
|
|
|
10-13
|
14-17
|
18-20
|
21-24
|
|
|
22-26
|
|
|
0.05-0.10
|
|
|
≥23
|
|
|
≤1.5
|
Viscosity (mpa.s) Concentration (1500mg/L)
degree of mineralization (5727m/L) Temp.(70℃)
|
≥8.5
|
≥10.5
|
≥11.5
|
≥12.5
|
Viscosity (mpass) Concentration (1000mg/L)
degree of mineralization (1000mg/L) Temp.(45℃)
|
≥30
|
≥40
|
≥50
|
≥60
|
Uses:
Used as oil displacement agent in tertiary recovery
Packing & storage
25kg paper-plastic composite bag, or following your demand. Its powder can adsorb the moisture and become the block matter, thus it should be kept in dry, cool and ventilating place. . |